This study evaluated the effectiveness of ultrasonic testing (UT) and magnetic particle testing (MT) for detecting weld defects to establish clear selection guidelines. The research was conducted using the Olympus OmniScan MX3 phased array UT system and GE Inspection MT equipment on carbon steel and stainless-steel samples containing intentional defects. The aim was to compare defect detection capabilities, analyze material property influences, evaluate operator technique impact, and provide a practical selection methodology. Results showed MT excelled at detecting surface cracks in ferromagnetic materials with 98.7% efficiency, while UT demonstrated superior performance for internal defects with 94.8% for subsurface cracks, 96.2% for porosity, 92.4% for lack of fusion, and 89.7% for slag inclusions. Material property analysis revealed a strong correlation between magnetic permeability and MT effectiveness (R²=0.9428), while UT performance showed moderate dependence on electrical conductivity (R²=0.8612). Operator experience significantly influenced accuracy, with UT improving by 0.47% per year and MT by 0.34% annually, resulting in 10.8% and 7.9% performance gaps between junior and senior operators respectively. The economic analysis showed UT equipment costs $85,000 (N140,250,000) with 4.5 m/hr inspection speed, while MT costs $15,000 (N24,750,000) with 8.2 m/hr speed. The study concluded with a comprehensive selection matrix specifying MT for surface defects in ferromagnetic materials and UT for all subsurface applications and non-ferromagnetic materials. These findings provide industry practitioners with evidence-based guidelines for optimizing weld inspection processes. Future research should investigate hybrid inspection methodologies and automated systems to reduce operator dependency, particularly for UT applications where human factors showed significant impact on inspection outcomes
GE Inspection, Magnetic Particle Testing Olympus Omniscan MX3, Operator Technique, Selection Matrix, Ultrasonic Testing, Weld Defects
Get Your e Certificate of Publication using below link
Preview Article PDF
Ebulogu Chidi Joel, Okwu Elemchukwu Isaac and Worgu Fortune. EVALUATION OF ULTRASONIC AND MAGNETIC PARTICLE TESTING FOR WELD DEFECT DETECTION USING OMNISCAN AND GE INSPECTION. World Journal of Advanced Engineering Technology and Sciences, 2026, 21(02), 110–124. Article DOI: https://doi.org/10.30574/wjaets.2026.21.2.0480